Screen printing is widely used to form metal contacts on solar cells, but the process can degrade device performance. The problem is particularly relevant to copper-plated silicon heterojunction (HJT) cells, which promise lower metallization costs and less reliance on silver. A research team in China investigated the degradation mechanism in these cells and tested a method to mitigate it, reporting the results in Solar Energy.
HJT cells depend on sensitive passivating contact structures. The mechanical pressure and thermal treatment involved in screen printing can damage those layers, raising recombination losses and lowering conversion efficiency. Understanding the damage pathway is therefore necessary for optimizing metallization without sacrificing cell performance.
Direct mesh contact during photoresist printing
Corresponding author Lang Zhou explained that printing photoresist for HJT cells differs fundamentally from conventional screen printing of silver paste. In silver paste printing, screen openings cover only 2–5% of the total area, while an emulsion layer covers the rest and prevents direct contact between the mesh and the wafer. Full-area photoresist coating typically uses a screen without emulsion coverage so that resist can be deposited uniformly across the wafer. As a result, the mesh contacts the wafer directly and extensively during every printing cycle.
The team said earlier investigations had shown conversion efficiency falling from 26.2% to 25.7% over 15,000 consecutive printing cycles in commercial solar cell production. Open-circuit voltage and fill factor accounted for most of the loss, while short-circuit current density and electrical resistance remained largely unchanged. Minority carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles.
Knuckle wear and hidden interface damage
Using three-dimensional confocal microscopy, the researchers identified progressive wear of the screen mesh knuckles as the main cause. As the knuckles wore down, their contact area with the wafer increased, placing greater mechanical stress on the passivation layers beneath. Scanning electron microscopy showed no visible surface scratches, but photoluminescence measurements indicated increased recombination losses. The researchers interpreted this as evidence of damage to the amorphous silicon/crystalline silicon interface.
Emulsion buffer and coating trade-off
To prevent direct contact between the mesh and the wafer, the team developed an emulsion buffer layer and evaluated six patterns with emulsion coverage ratios from 2.9% to 16.6%. The results revealed a trade-off: greater emulsion coverage reduced mechanical damage but impaired photoresist coating uniformity and ink distribution. A coverage ratio of 4.7% provided the best balance, limiting minority carrier lifetime degradation to 0.41% after 10,000 printing cycles while maintaining relatively good coating uniformity.
The researchers attributed the improvement to the emulsion layer blocking direct contact between the screen mesh and wafer, thereby reducing cumulative mechanical damage to the sensitive passivation layers. Zhou said the findings show that a relatively simple change to screen design can substantially mitigate printing-induced degradation, offering a practical route to improving manufacturing reliability for copper-plated HJT cells.
Copper metallization gains attention
The work comes amid growing interest in copper as an alternative to silver contacts in HJT cells. In April 2026, researchers at China’s Nankai University reported a silver-free HJT cell with 25.2% efficiency using plasma-induced interface engineering and copper electroplating. That approach addressed adhesion, contact resistance and stability challenges at the indium tin oxide interface.
Separately, scientists at Germany’s Forschungszentrum Jülich achieved 23.08% efficiency in a fully copper-metallized HJT cell. The silver-free device showed a relatively small efficiency penalty compared with its silver-metallized counterpart, while cells combining silver-copper paste on the front side with silver contacts on the rear reached 23.95%. Those results underline copper’s potential to reduce silver consumption, although further improvements in processing and electrical performance are still needed.